Sut i Weithredu 2 Mewn 1 Peiriant Dosbarthu&boglynnog?

Jun 13, 2018

Gadewch neges

27-1.jpg


ProcessofEmbossing

1.Setthepositionformoldsyouwillsticktotheheatingplaten.
2.Preheatthemachine.Setthetemperaturebetween220-235 ℃ .andthetimeabout8sec.
3.Maketheheatingplatenpressdown.After8sec.itwillautorelease.
4.Usethemachinetodotheembossing.Butbeforedoingembossing, youneedtoknowthereisthestepthatscrapethesilicone (aswellasscreenprinting) onthepiecesfabric.

ProcessofSilicone

1.Preheatthemachine.Settimeabout170-220 ℃.
2.Mixcolorliquid, curingagentandthesiliconetogetherinproportion.
3.putthemintothevacuummachinetolettheairgoout.
4.scrapetheitemsonthemold.Finally, youcanpressit.

27-2.jpg


Os hoffech chi gael yr effaith silicon, bydd angen y peiriant gwactod arnoch chi.

Gobeithio y bydd yr wybodaeth uchod yn ddefnyddiol i chi